• Aqueous solution of polymeric dispersion, enriched with quartz sand of selected granulometry and special improving additives.
• Aqueous solution of polymeric dispersion, enriched with quartz sand of selected granulometry and special improving additives.
• The substrate must be firm, dry and clean. • Before the application, the contents of the plastic container must be thoroughly stirred. It can be diluted with up to 20% water. In case of dilution, it is recommended that the contents are consumed within 2-3 days. Within these time limits, the separation of the phases, after dilution, does not affect the properties of the product. In this case, good stirring is recommended. • It is applied to the surfaces with a roller, a brush or with the special automatic spraying device. • The coated surface is ready for plastering after drying for 4 to 8 hours depending on the weather conditions and the type of substrate. • The application temperature should be between +5 oC and +35 oC.
• In containers of 17 kg and 4 kg in pallets. • In sealed containers and in a dry environment, protected from frost and prolonged exposure to strong sunlight for 12 months from the date of production.
Approximately 250-350 gr/m2, depending on the thickness of the layer, the dilution and the type of substrate.
Form Paste Granule size | 0.0-0.7 mm |
Density | 1.40 kg/l |
Consumption | 250-350 gr/m2 |
pH (ISO 787-9) | 8-9 |
Adhesion (EN 24624:2003) | 0.5 MPa |
Water absorption (EN 1062-3:2001) | 0.47 kg/m2 .min 0.5 |
Vapor permeability (EN ISO 7783-2:2001) | <13 gr/(m.d) → Sd<0,16 |